Pin-in-Paste Soldering: Through-Hole Reflow Design Guide

By Published On: September 12th, 2024Categories: Blog, PCB Assembly

Table of Conent

Table of Conent

Pin-in-paste soldering places through-hole component leads into printed solder paste and forms the joints in a reflow oven. Also called through-hole reflow (THR) or intrusive reflow soldering, it can combine selected through-hole parts with surface-mount assembly. It is suitable only when the component, PCB geometry, paste deposit, insertion method, and measured thermal profile work together. A conventional through-hole connector is not automatically a reflow-compatible connector.

The practical decision is whether each joint can receive enough solder and reach its qualified soldering conditions without exceeding the limits of the connector or neighboring components. Removing a separate soldering operation can be useful, but it does not justify accepting unstable filling, damaged housings, or repeated touch-up. Review the complete PCB assembly process before choosing the route.

Updated November 4, 2026. Product drawings, supplier process instructions, and the agreed assembly acceptance requirements govern the actual build.

How the Pin-in-Paste Process Works

The basic sequence is paste printing, component insertion, reflow, and joint verification. Each stage must preserve the material needed for the final through-hole joint. Paste visible below a pin after insertion is not, by itself, proof of either a good joint or a defect.

  1. Print the planned paste deposit at the plated through-hole locations and the associated surface-mount pads.
  2. Place the surface-mount components and insert the approved THR parts in the validated sequence.
  3. Reflow using a profile demonstrated on the populated assembly, including its thermally demanding locations.
  4. Inspect the resulting joints and reconcile any missing solder, bridging, or component damage with the earlier process evidence.

For the physical mechanism, Phoenix Contact’s THR explanation describes how paste displaced around a pin can melt and return toward the hole. Its discussion also identifies pin protrusion as an important influence. Treat the insertion result as something to qualify, rather than assuming all displaced paste will return to the barrel.

Illustration of the pin-in-paste sequence with evidence checks after printing, insertion, reflow, and inspection
Illustration: four stages and the evidence to retain. This is a process review map, not a production record.

Check Component and PCB Suitability First

Start with a documented THR-capable part and a tolerance review. Hole diameter, pin cross-section, board thickness, lead length, and housing clearance affect both assembly and solder demand. Making the hole as small as possible is not a complete design rule.

Harwin’s termination-method comparison explains that reflow exposes the whole connector to heat. Check the exact part number and supplier limits, not just a plastic material name or the temperature rating of a related family. Confirm permissible process exposures and any handling restrictions before approving an alternative component.

Inputs to resolve before a pin-in-paste trial
Input Question to resolve Evidence to retain
Component Is this exact configuration approved for the intended reflow conditions? Part number, drawing revision, supplier soldering limits
Pin and finished hole Do tolerance extremes permit insertion while keeping solder demand practical? Pin dimensions, finished-hole tolerance, board thickness
Housing and lead length Can insertion displace paste without trapping it under the body or losing it? Standoff, protrusion, underside clearance, insertion observation
Nearby features Can the deposit fit without feeding exposed copper or adjacent joints? Land pattern, solder mask, neighboring pads and vias
Thermal conditions Can all relevant joints reflow within every affected part’s limits? Measured profile, sensor locations, supplier limits

Use finished-hole dimensions rather than the drill tool diameter when evaluating the space around a pin. For a non-round lead, use its actual cross-sectional geometry for volume calculations and its limiting dimensions for insertion clearance. Check tolerance combinations; nominal dimensions alone can hide an assembly interference or a large solder-volume requirement.

Keep annular lands and solder mask consistent with the released PCB design and fabrication requirements. Do not shrink lands solely to reduce solder demand. Separate intended solderable features from unrelated exposed copper in the deposition area, and resolve clearance under the connector before increasing the deposit.

If the selected connector or footprint makes the route uncertain, share the connector drawing and affected board geometry, together with the BOM and intended assembly sequence, so the component and tooling constraints can be reviewed before a stencil is ordered.

Balance Solder Volume and Pin-in-Paste Stencil Design

The deposit must supply the required solid solder after reflow, while remaining printable beside the SMT features. Wet paste volume and final solder volume are different quantities. A paste’s metal percentage by weight must not be substituted for its metal fraction by volume.

A useful geometric starting point is the empty barrel space: hole cross-sectional area minus the pin cross-sectional area, multiplied by board thickness. Include the planned fillets when estimating the joint’s solder demand. AIM’s pin-in-paste technical paper explains this joint-volume approach and the conversion to paste volume. Use the actual formulation’s information and the required joint geometry; the calculation is a planning estimate, not proof of acceptable barrel fill.

For a hypothetical comparison, keep the pin and board thickness unchanged and enlarge only the hole. The unoccupied barrel volume increases, so more solder must be delivered. That does not mean the larger aperture needed to deliver it will fit between neighboring components. This simple comparison helps identify when a footprint change is more useful than a printer adjustment.

Indium’s aperture-design example illustrates how excessive hole-to-pin clearance can create an impractical paste requirement. Its example dimensions are specific to that problem. Do not transplant them as a universal hole clearance or stencil recipe.

Evaluate overprinting, local stencil thickness changes, or another qualified solder-supply method against the surrounding layout. A thicker stencil chosen for a connector can overdeposit paste on nearby fine-pitch pads. A larger opening can also interact with the housing, solder mask, or adjacent exposed features. Establish the deposited quantity and its repeatability, rather than relying only on the calculated aperture volume.

Illustration separating required solid solder volume, wet paste demand, local deposition space, and trial verification
Illustration: translate joint demand into a feasible deposit, then verify it. No universal volume factor or aperture dimensions are implied.

The separate vacuum packer PCBA example addresses the product-specific conflict between fine-pitch SMT and larger pin-in-paste deposits. This guide covers the general route-selection and qualification questions.

Qualify Printing, Insertion, and the Thermal Profile

Qualification needs evidence from the populated board, not an oven setpoint or one attractive solder fillet. Control the paste, stencil revision, print program, support arrangement, component seating, and insertion sequence so a trial can be repeated.

A fixed squeegee angle is not a universal solution to through-hole filling. Begin with compatible printer, stencil, and paste recommendations, then compare justified changes while retaining the baseline. For print-stage symptoms, the solder paste printing defect guide provides a separate investigation framework; it does not replace the THR joint-volume review.

Observe what insertion does to the deposit. Record bent pins, incomplete seating, paste carried away on long leads, and material trapped beneath the housing. If these change between trials, an apparent improvement after reflow may not be attributable to the parameter being tested.

Würth Elektronik’s THR connector application note identifies component heat tolerance, heat access to solder locations, and component handling as design considerations. Its connector example reinforces why the measured result must match the actual assembly configuration.

Agree on sensor locations and record how the profile was measured. Compare relevant joint temperatures with the paste’s process guidance and component limits. Review thermally demanding connector locations and temperature-sensitive parts together. A profile that works for an isolated component does not establish the same result next to a large plane or a different population.

Define inspection coverage before the trial. Visible external fillets alone do not reveal all internal barrel conditions. Select an appropriate inspection approach for the geometry and requirements, with additional examination where necessary. Record the applicable acceptance document, revision, product class where relevant, sampling plan, and any customer requirements; do not use one generic fill percentage as the release rule for every assembly.

Benefits, Limits, and When to Keep a Separate Soldering Step

Pin-in-paste can remove a separate through-hole soldering operation when the selected parts and joints are compatible with the SMT flow. Compare the complete route, including tooling, insertion, inspection, rework, and expected build quantity. Fewer named process steps do not automatically produce a lower total assembly cost.

Questions that can change the assembly route
Finding Implication Next decision
Part lacks documented reflow compatibility The proposed shared reflow route is not established Review an approved alternative or a separate soldering operation
Required deposit conflicts with nearby SMT pads A uniform stencil may not meet both needs Review local tooling, solder supply, or the footprint
Joint heating conflicts with another part’s limits The shared thermal window may be infeasible Review sequence, component choice, or separate processing
Repeated touch-up dominates the trial Nominal step reduction may hide added cost and variation Compare the full qualified routes before release

Keep the trial record tied to the actual board, BOM, paste, stencil, program, and component revisions. Review substitutions against the same constraints. A successful prototype demonstrates the tested configuration; it does not automatically qualify every pin length, housing option, or production restart condition.

Frequently Asked Questions

Is pin-in-paste the same as press-fit assembly?

No. Pin-in-paste uses solder and reflow to form a joint. Press-fit uses a qualified mechanical interference connection. Select the process specified for the exact connector and board interface.

Does intrusive reflow soldering eliminate every later soldering operation?

No. Other components may still require a different route. Evaluate the complete BOM and assembly sequence before claiming a single-pass build.

Can an existing stencil be reused after a connector substitution?

Only after reviewing the changed pin geometry, footprint, housing clearance, and process limits. Retain the comparison and any required trial evidence with the substitution approval.

Successful pin-in-paste soldering depends on a compatible component, a feasible deposit, controlled insertion, and verified joint formation. For a mixed-technology build, provide the fabrication and assembly package with the THR constraints, including Gerber files, BOM, placement data, connector drawings, quantity, and test requirements, so OrinewPCB can review the manufacturing scope and the proposed assembly route together.

Latest Blog

Contact Info

Phone: +86-755-82882936

Email: [email protected]

WhatsApp: +86-13570802455

Wechat: +86-13570802455

Address: 2nd floor,D Bldg.,Electric Link Technology Bldg.,Gongming,Guangming New Dist.,518106 Shenzhen, China

Free Quote

Click or drag a file to this area to upload.

Share This Post!